Paul
Actually, we no longer use dye, per say. We use the stuff machinists use for
staining metal. Look here for hints:
* <http://www.ivf.se/Elektronik/dye_penetrant/edefault.htm>
* <http://www.amkor.com/products/notes_papers/SMTAI_2000_Darveaux.pdf>
* Dye-and-pry failure analysis (technique described in B. Mullen, A. Hertz,
B. Miles, and R. Darveaux ["Plastic Ball Grid Array Assembly," Ball Grid
Array Technology, J. Lau Editor, McGraw-Hill, Inc., New York, 1995])
* Process Sciences Inc [ http://www.process-sciences.com ] wrote a
newsletter, fairly recently, with a section on dye & pry.
This is a messy process [and there is no return]. What are you looking to
clean?
Dave Fish
----- Original Message -----
From: "Stolar, Paul W" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, February 17, 2004 4:35 PM
Subject: [TN] Dye
> Does anyone have experience with dye penetrant on assembled PC boards?
>
> Questions are:
> 1. any special dye?
> 2. how to clean?
>
>
> Paul Stolar
> Materials/Reliability Engineer
> Manufacturing Reliability Lead Engineer
> Baker Atlas
> 713-625-5376
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
> -----------------------------------------------------
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|