This may be the AVX paper that John Maxwell spoke of:
www.avxcorp.com/docs/techinfo/soldpad.pdf
Dave Fish
----- Original Message -----
From: "John Maxwell" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, February 24, 2004 5:54 PM
Subject: Re: [TN] Skewed Components
> Hi Steve,
> Three things are contributing to skew;
> 1) pads are too wide
> 2) A bit too much solder
> 3) Overlap to extension ratio is >>1
>
> For example we found during a study a decade + ago that component movement
> and resulting defects like a tombstone or drawbridge were a minimum when
> the length of a chip resting on the pad equaled the extension of the pad
> beyond the end of the termination. Another factor is that you have this
> condition optimized when overlap(O) = extension (E) = nominal termination
> band length (T). Defects sort of disappeared when stencil thickness and
> corresponding volume of solder was reduced over the years but leapt back
> into the fray with really small chips like 0603/0402/0201 came into common
> use.
>
> The simple solution is reduce the stencil aperture to where you want the
> parts to stay (plus a little for luck) and have at it. You probably have
> enough solder already just in the HASL board finish for a reliable solder
> joint so stencilled solder paste is will be supplying the flux.
>
> I don't know if that paper is still on the AVX web site but the data was
> generated when IPC-SM-782 was first being formulated and that started in
1984.
>
> Nice photo.
>
>
>
> John Maxwell
>
>
> At 05:33 PM 2/24/2004 -0500, you wrote:
> >Hi All!
> >
> >Got a little issue here that I need to dig in deeper to, but I thought
I'd
> >post a picture on my web page and ask for your valued opinions. Was
building a
> >board today that we've built before, never had any problems with it. But
today
> >certain 0805 resistors started skewing on their pads during reflow, and
I
> >don't know why. Take a look at:
> >http://www.stevezeva.homestead.com and look at "skewed components". It's
not
> >really a defect because they're 100% on the pads, and the wetting and
fillets
> >are fine too. They just look funky...and this just started happening. Not
so
> >much as a pimple on the boards before when we built them.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest