Hello,
I've got some bare boards (.062 thick, double sided, LPI, HASL) that appear
to have "solder smear" on them. That is, random areas of what certainly
appears to be solder adhered to the soldermask in areas where there aren't
pads or traces.
I sent a couple samples back to the boardhouse, and they believe it is a
burnishing of the mask from contact pressure, not an area of a thin solder
coating as we believe it to be.
What test method should I use to verify what we are seeing?
TIA,
Hal
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|