Werner, at least we agree, even if you pipped me to the post by a few
minutes! :-)
Brian
Werner Engelmaier wrote:
> Hi Rudy,
> Your explanation sounds good, but is incorrect--it is not the surface
> roughness that is the problem, it is the variability of the ED copper density. The
> specific gravity (density) of ED copper is less than the specific gravity
> (density) of rolled copper because of organic co-deposits and micro-voids. This
> uncertainty in specific gravity (density) prevents a direct conversion of oz./ft2
> to thickness, and that is why ED copper is specified in oz./ft2.
> The reason weight is used in specifying copper foil is because copper is
> bought and sold by weight.
> So, foil vendors sell copper foil by weight; the laminators resell the foil,
> laminated to epoxy, by area. Want to guess how much foil is produced near the
> upper weight tolerance for any given foil weight class?
> None of thus of course excuses the lazy stupidity in this country that has
> killed the use of the metric system time and again.
>
> Regards,
> Werner Engelmaier
> Fornercahairman of IPC Copper Fopil Committee
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
>
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|