Depends on what material the board is coated with. Dynaloy has some removers that we have had success in using on several different urethanes without damaging components.
Chris Almeras
Diversified Systems
-----Original Message-----
From: Dave Girard [mailto:[log in to unmask]]
Sent: Monday, June 02, 2003 8:58 AM
To: [log in to unmask]
Subject: [TN]
What is the best process and chemical to use to strip urethane conformal
coating from plastic bodied surface mount components.
Dave
David N. Girard
David N. Girard, CQE, CQA, NCE
Senior Reliability Engineer
Honeywell
Aerospace Electronic Systems
Defense & Space Electronics
Clearwater Defense
13350 U.S. Highway 19 North
M.S. 322-4
Clearwater, FL 33764-7290
Phone: (727) 539-2018
Fax: (727) 539-4991
E-Mail: [log in to unmask]
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|