Depends on what material the board is coated with. Dynaloy has some removers that we have had success in using on several different urethanes without damaging components. Chris Almeras Diversified Systems -----Original Message----- From: Dave Girard [mailto:[log in to unmask]] Sent: Monday, June 02, 2003 8:58 AM To: [log in to unmask] Subject: [TN] What is the best process and chemical to use to strip urethane conformal coating from plastic bodied surface mount components. Dave David N. Girard David N. Girard, CQE, CQA, NCE Senior Reliability Engineer Honeywell Aerospace Electronic Systems Defense & Space Electronics Clearwater Defense 13350 U.S. Highway 19 North M.S. 322-4 Clearwater, FL 33764-7290 Phone: (727) 539-2018 Fax: (727) 539-4991 E-Mail: [log in to unmask] --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------