TECHNET Archives

March 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Phil Nutting <[log in to unmask]>
Date:
Tue, 4 Mar 2003 10:08:16 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Grabski III, John R." <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Grabski III, John R." <[log in to unmask]>
Parts/Attachments:
text/plain (114 lines)
With a tinned wire, pull test results will be all over the place, due to the
wire resting in different spots in the termination piece to piece...

Get ahold of MIL-T-7928...  good ring terminal bible.  Regardless of the
make, we subject all UL and MIL ring terminals in house to MIL-7928 test
criteria.

... doesn't 610-B also have some info on this subject?

-John Grabski III
Eng. Dept.
Badger Technologies, Inc.
www.badgertech.com

 -----Original Message-----
From:   Phil Nutting [mailto:[log in to unmask]] 
Sent:   Tuesday, March 04, 2003 10:00 AM
To:     [log in to unmask]
Subject:        Re: [TN] tined wire with insulated lug

Jean-François,

This is something I brought up back in May of 2002.  Look for "Crimped
Connections" in the subject line. There should be about 12 posts following
this thread in the Archives.

To add more input, I have a document from Amp (now Tyco) Engineering stating
that pre-tinning stranded wire before crimp termination is not acceptable.
I can send it to you if you'd like.

I've had to battle the "we've always done it this way" attitude along with
the notion that they are running "a lot of current" through the connection.
My answer to that is, hope you're not running more current than the pin or
lug was designed for.

Good luck,

Phil Nutting

-----Original Message-----
From: Bissonnette, Jean-Francois [mailto:[log in to unmask]]
Sent: Tuesday, March 04, 2003 9:02 AM
To: [log in to unmask]
Subject: [TN] tined wire with insulated lug


Hi All,

I'm trying to find acceptance criteria for crimped lugs.  Is it acceptable
to have a pre-tined wire
crimped in a ring terminal?  Since the wire is tined, it won't compress as
much as it would if wasn't.
Can that cause reliability problems?

Jean-François Bissonnette
Vérificateur, Contrôle de la Qualité
Électronique
Produits et Procédés
Vapor Rail Inc.
10655 Henri-Bourassa O.
St-Laurent, Qc
H4S 1A1

(514) 335-4200 x2021
(514) 335-4231 fax



***** CONFIDENTIALITY NOTE *****
The content contained in this e-mail transmission is legally privileged and
confidential information intended only for the use of the individual or
entity named herein. If the reader of this transmission is not the intended
recipient, you are hereby notified that any dissemination, distribution, or
copying of this transmission is strictly prohibited.

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2