What type of end termination is on the cap? I assume a 3 or 5 face. Wow, how could this have missed or unnoticed?
Kat
>>> [log in to unmask] 02/13/03 08:17AM >>>
I got one more info that may confirm the source of my problem,
maybe some of you can confirm.
The lands for the capacitors are too close together and probably
not wide enough. Seems like the land patern is so that it fits the
cap's width and the end comes flush with the cap at the ends.
Results, there is no solder fillet neither on the end nor on the sides.
Any thoughts?
***** CONFIDENTIALITY NOTE *****
The content contained in this e-mail transmission is legally privileged and confidential information intended only for the use of the individual or entity named herein. If the reader of this transmission is not the intended recipient, you are hereby notified that any dissemination, distribution, or copying of this transmission is strictly prohibited.
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
<!DOCTYPE HTML PUBLIC "-//W3C//DTD HTML 4.0 Transitional//EN">
<HTML><HEAD>
<META http-equiv=Content-Type content="text/html; charset=iso-8859-1">
<META content="MSHTML 6.00.2715.400" name=GENERATOR></HEAD>
<BODY style="MARGIN-TOP: 2px; FONT: 8pt MS Sans Serif; MARGIN-LEFT: 2px">
<DIV>What type of end termination is on the cap? I assume a 3 or 5
face. Wow, how could this have missed or unnoticed? </DIV>
<DIV> </DIV>
<DIV>Kat<BR><BR>>>> [log in to unmask] 02/13/03 08:17AM
>>><BR>I got one more info that may confirm the source of my
problem,<BR>maybe some of you can confirm.<BR><BR>The lands for the capacitors
are too close together and probably<BR>not wide enough. Seems like the
land patern is so that it fits the<BR>cap's width and the end comes flush with
the cap at the ends.<BR>Results, there is no solder fillet neither on the end
nor on the sides.<BR><BR>Any thoughts?<BR><BR>***** CONFIDENTIALITY NOTE
*****<BR>The content contained in this e-mail transmission is legally privileged
and confidential information intended only for the use of the individual or
entity named herein. If the reader of this transmission is not the intended
recipient, you are hereby notified that any dissemination, distribution, or
copying of this transmission is strictly
prohibited.<BR><BR>---------------------------------------------------<BR>Technet
Mail List provided as a free service by IPC using LISTSERV 1.8e<BR>To
unsubscribe, send a message to [log in to unmask] with following text in<BR>the
BODY (NOT the subject field): SIGNOFF Technet<BR>To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL)<BR>To receive ONE mailing per day of all the posts: send e-mail
to [log in to unmask]: SET Technet Digest<BR>Search the archives of previous posts
at: <A
href="http://listserv.ipc.org/archives">http://listserv.ipc.org/archives</A><BR>Please
visit IPC web site <A
href="http://www.ipc.org/html/forum.htm">http://www.ipc.org/html/forum.htm</A>
for additional<BR>information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700
ext.5315<BR>-----------------------------------------------------<BR></DIV></BODY></HTML>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|