Hi Technetters,
We're having problem with some multilayer ceramic capacitors (SMT), they
crack. We have a
high level of rejects from the field and we're thinking of replacing them.
However, the
best that the design team came up with so far is to use regular ceramic
capacitor (TH)
(... please don't ask why they don't chance supplier... I already did and
well, forget it!)
I'm not too confortable with that, but on the other hand, a design change on
the board
would be very costly and we want to avoid that.
Did anyone ever changed a SMT part for a TH part? What problems should we
expect
if we decide to go that way? Of course assuming that the leads would be
bent properly, the
cap would be bonded to the board, every applying rule for soldering would be
respected and
Murphy won't show its ugly face... then again we all know what appends when
we assume...
I'd prefer to go another way but my way will cost a lot of money and I'm
told that we have to
keep it to a minimum.
Any thoughts?
Jean-François Bissonnette
Vérificateur, Contrôle de la Qualité
Électronique
***** CONFIDENTIALITY NOTE *****
The content contained in this e-mail transmission is legally privileged and confidential information intended only for the use of the individual or entity named herein. If the reader of this transmission is not the intended recipient, you are hereby notified that any dissemination, distribution, or copying of this transmission is strictly prohibited.
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|