It would depend on the finish, how it was applied, the process involved, how
they were handled after that process, how they were packaged, and how they
were stored...
My guess is anywhere from a day to 10 plus years...seriously...I found a
package of boards built 10 years ago, in a drawer we were cleaning out,
thought it would be interesting to see the results so we soldered
them...turned out great...so a note to everyone, store your boards in desk
drawers of air conditioned offices cleaned nightly by an outside service...
So what type finish are you talking about, and how are they packaged...
Franklin
----- Original Message -----
From: "Bissonnette, Jean-Francois" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, January 29, 2003 2:54 PM
Subject: [TN] Shelf life of PWB
What is the shelf live of a PWB. After how long can I expect to have
solderability problem?
Thanks!
Jean-Frangois Bissonnette
Virificateur, Contrtle de la Qualiti
Ilectronique
Produits et Procidis
Vapor Rail Inc.
10655 Henri-Bourassa O.
St-Laurent, Qc
H4S 1A1
(514) 335-4200 x2021
(514) 335-4231 fax
***** CONFIDENTIALITY NOTE *****
The content contained in this e-mail transmission is legally privileged and
confidential information intended only for the use of the individual or
entity named herein. If the reader of this transmission is not the intended
recipient, you are hereby notified that any dissemination, distribution, or
copying of this transmission is strictly prohibited.
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|