Ong:
There is a tool that resembles a comb that measures wet thickness.
One of the companies that carries it is Nordson, a company that manufactures
CC spraying machines.
Good luck, Ramon
> -----Original Message-----
> From: Ong Seet Leng [SMTP:[log in to unmask]]
> Sent: Thursday, January 23, 2003 9:51 PM
> To: [log in to unmask]
> Subject: [TN] ADVISE NEEDED
>
> Morning Technetters,
>
> Advise needed. We used to use dipped in method using a conformal coating
> machine but as the latex used to cover the forbidden area need at least a
> few hours to cure, we cannot afford the time. Due to the extremely tight
> schedule given to us, we have engineers sending in assembled boards in the
> morning and expect us to perform miracles and have them ready before
> lunch.
>
> We are now using the hand brush method but as mentioned, due to the
> extremely tight schedule, is there any way to measure the coating
> thickness without say, measure assembled board before coat, after that
> coat one side-measure again, before coat the other side & measure again in
> order to get the individual side coating thickness?
>
> We may have used the wrong approach and I desperately need some advise
> from you guys and gals. More over, should we revert back to dip in method,
> how are one going to measure the coating thickness of one side and then
> protected it before proceed to the un-coated side? Any suggestions is
> greatly appriciated.
>
> Regards
> S L Ong
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|