Margaret,
If this is a standard 5-sided cap, you can find the req's in IPC-A-610 sec
12.2.2. From what you describe, your rework operators are simply adding
solder to the land area to form a bridge between the part and the land, this
is then call drawbridging and may meet the minimum req's although not be the
most reliable due to the differring forces pulling on the component during
thermal cycling.
If you want to rework the parts and have the right equipment and training,
assuming you have the same amount of solder on both sides of the component
pasted and reflowed, you can have your operators flux both sides of the site
and reflow with a hot air pencil to level the part. This will introduce
less thermal shock to the component if that is a concern of yours, if not,
use a pair of thermal tweezers and do the same.
Bill Westmoreland
President, BEST, Inc.
www.solder.net
Phone (847) 797-9250
Fax (847) 797-9255
Email [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of gosia
Sent: Wednesday, January 08, 2003 8:54 PM
To: [log in to unmask]
Subject: [TN] Help anyone!!!
Hello TechNet,
Please help!!!
Recently, we have a problem with tombstone components. Operators
were told to repair them by adding solder to the lifted side of the
caps, so there is a solder connection but the side remains lifted .
In my opinion this is not an acceptable condition because the capacitors
do not meet the requirements of dimension J - Minimum End Overlap. The
other Quality Inspector disagrees on the bases that connection has been
made by solder.
Where can I find specific standards for lifted SMT capacitors?
Margaret
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|