TECHNET Archives

January 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 23 Jan 2003 10:51:35 EST
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="ISO-8859-1"
From:
Werner Engelmaier <[log in to unmask]>
Parts/Attachments:
text/plain (44 lines)
Hi Howard,
I have never seen: Spec Number TSC7514g, section 5.4, reference specification 
TSC 7010g, or anything like it, and I have been involved in SMT reliability 
for almost 25 years. 
>The first question is: is this customer using their own test or is there an 
>IPC test for thermal cycling of a completely assembled circuit board?
ANSWER: The test (Ts, dwell times) is reasonable, except for its use of 
thermal shock--T-shock will give you totally misleading results, because the 
high T-gradients cause component and PWB warpage, and thus create tensile 
loads not seen in product. Further, a different damage mechanism in the 
solder [see Günter's response] occurs due to the much higher stress levels 
occurring with T-shock. For test guidelines and a standard go to IPC-SM-785 
and IPC-9701.

>The second question is: is the customer's temperature range too extreme,
>which is causing severe thermal shock, which is then causing joint failures
>due to different co-efficients of expansion and contraction  (board, solder,
>lead)?
ANSWER: For T-cycling, the Ts are not extreme. For T-shock the differences in 
CTEs are not as much of a factor as are the T-gradients.

>The third question is: is the use of 3,500 hours of thermal cycling realistic
>and/or too long?
ANSWER: For T-cycling no--all bets are off for T-shock.

Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL  32174  USA
Phone: 904-437-8747, Fax: 904-437-8737
E-mail: [log in to unmask], Website: www.engelmaier.com 

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2