Hi Tom,
Unfortunately, the info you provided is not complete enough to be more
definitive, however...
(1) Your failures are definitely caused by the thermal expansion mismatch of
the copper barrels and the surrounding reson volume;
(2) The affected vias were more suspectible to failure because they may
(a) have seen higher and/or more often T-excursions [manual soldering];
(b) had localized stress-riser defects [remember, a X-section sees only 2
points of the 360° barrel circumference], that started cracks during
soldering proces[ses] which propagated to completion in subsequent burn-in
and operational use---the stated "the epoxy appeared to
have a small crack also in the same plane as the barrel crack" indicates a
possible drilling quality problem causing glass-fiber rip-out which than
causes a localized plating defect which raises the effective maximum strain
on the Cu barrel [see IPC-D-279];
(c) significant dog-boning has occurred;
(d) the physical properties of the ED barrel copper is inadequate.
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 904-437-8747, Fax: 904-437-8737
E-mail: [log in to unmask], Website: www.engelmaier.com
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|