Hi! can someone help,
we are doing flexible PCB with the Nickel/Gold
finishing,we facing the gold peeling from gold to
nickel peeling problem recently on certain plating
panels
Normally, we use plating rack for gold plating,
every loading is 4 panels. The gold peeling pattern
is total 4 panels per same loading will have gold
peeling,some loading don't found any gold peeling.
Is this mean the plating rack have problem?
1] In term of chemistry, what kind of situation the
specific chemical can cause this problem?
2]In term of nickel passivation; what should be the
possible cause? How to identify the root cause of
nickel passivation? Is it only happen on cartain
period during different panel loading?
3]Why only certain loading have the gold peeling
problem & others do not?
4]If water rinse is the main cause of nickel
passivation? What is the deionize water quality
requirement? How far is the flow rate affected the
nickel passivation?
5]Whether the plating current cause the gold
peeling from nickel? How this heppen?
6]May this cause by the gold plating bath
chemistry? If the chemical parameter within spec.;
what else can cause the problem?
Please help on this. Thank you.
Regards,
Dev
__________________________________________________
Do you Yahoo!?
Yahoo! Mail Plus - Powerful. Affordable. Sign up now.
http://mailplus.yahoo.com
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|