Hi Poh,
Do you use active flux during touch up ?
If you do, it can be that your board is not clean. In that case, flux can
help.
Try touch up with out flux and compare.
It seems that your Reflow profile - OK, because you have good solder fillet
from outlook. It could be a simple solderability problem
Happy new year
Eli
----- Original Message -----
From: "pohkh" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Saturday, December 21, 2002 3:34 AM
Subject: [TN] : Dry Solder ?
> Hi,
>
> Can someone help me to understand why the good solder
> fillet from the appearance, but detected to be opened
> when performed testing.
>
> From X-ray, there is no evidence of open joint. Once
> we touch up, it passes the test.
>
> We tend to see this kind of symptom rather common.
>
> It seems that the good solder fillet from outlook,
> does not mean a good electrical solder joint.
>
> Is there way to solve this symptom.?
>
> Thanks.
>
> Regards,
> Poh
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|