TECHNET Archives

August 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Earl Moon <[log in to unmask]>
Date:
Wed, 28 Aug 2002 10:19:09 +0800
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Content-type:
text/plain; charset=iso-8859-1
Subject:
MIME-Version:
1.0
Content-transfer-encoding:
quoted-printable
From:
Parts/Attachments:
text/plain (149 lines)
I think what victor referring was the die attach solder fillet (with
respect to the thickness of the die).
I think bondline thickness of the die attach should be a range of 1-1.5
mils (with less than 10 % voids over the die area).
The fillet of the solder should not be more than 50% of the die thickness.
Some Die attach machines
can achieve ±2 mils placement tolerance. Some Customers require that
tolerance for SMT.

regards
JONOQs



                                                                                                                                       
                      Earl Moon                                                                                                        
                      <[log in to unmask]        To:       [log in to unmask]                                                               
                      M>                       cc:                                                                                     
                      Sent by: TechNet         Subject:  Re: [TN] Die attach/bonding material                                          
                      <[log in to unmask]>                                                                                                
                                                                                                                                       
                                                                                                                                       
                      08/28/02 03:44 AM                                                                                                
                      Please respond to                                                                                                
                      "TechNet E-Mail                                                                                                  
                      Forum."; Please                                                                                                  
                      respond to Earl                                                                                                  
                      Moon                                                                                                             
                                                                                                                                       
                                                                                                                                       




Victor,

I'm not posting this to embarass you but to point out how much your are
doing and why:

Victor,

I mean this in a very complimentary way. How do you do so much? I mean are
you the only one left like you at Dell doing this stuff all the way from
chip level stuff design through customer acceptance. I really admire all
you
do and all the questions you ask.

For this particular question, I yield to more knowledgeable die attach and
wire bonding technology experts though I have done a bunch of it, I'm just
not current. Also, I don't completely understand the questio relative to
how
far up the thickness of the die can the bonding material cover.

ISHM, or whatever it is now called - just can't remember at the moment,
should have many answers to your questions as would some semiconductor
forume.

Regards,

Earl MoonMan



Victor,

I hope you receive more responses too. Thanks for the insight. Since your
first postings I couldn't figure out what you were doing, especiall with
Dell. Now I get it.

Having spent another life with IBM, I can only imaging how you can help
Dell
even if a bit after the fact. F/A is fun especially when findings get
routed
back to designs. Hell, I might even buy a big black box now knowing what
your doing.

Sorry I could not have been any real help. I have lots of die attach and
wire bond experience but haven't used it in some time. I know you will find
your answers.

Enjoy,

Earl


   I am here not by choice but after Big Blue/Multek_Austin went belly up.
This is the closes to an FA Lab that I will get a chance to used my skills
after many years of practice.   In the previous years I did the cross
section
and gave the findings to an engineer who wrote the report.   Now I have to
do
all the wrap up.   That I why I don't recall the reference requirements.
I
known it exists some where's.   We all have to make a living till we quite
paying taxes and add iron to the earth.

victor,



Victor,

You're one hard woking guy. The experience you are gaining now will take
you
far probably without adding ferrous metals to the eart's much too shallow
crust. I think you have some time to go for that.

Keep up the great work and let us know some of it turns out. Hell, write a
book - when you find time.

Earl


I have followed this gentleman's post for some time. I am impressed at the
knowledge this many is trying to attain and, for all the right reasons, use
it.

I'm impressed and tired just trying to keep up

MoonMan

---------------------------------------------------------------------------------

Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------



---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2