Hi Joyce,
It may help if the manufacturer of the heat sink starts with 1.0 cm stock
instead of starting with thicker Cu stock and machine it down to 1.0 cm. I
do not know how practical is that and what surface finish the heat sink
should have. But it may be worth trying.
Sherif,
----- Original Message -----
From: "joyce" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, July 11, 2002 8:16 AM
Subject: [TN] warpage heat sink
> Guys,
> I got a heat sink look like potato chips after reflow using conduction hot
> plate (230-240 C). The heat sink is 1 cm thick Cu with few position screw
> holes on 2 sides. The size is 13.0x10.0x1.0 cm with 0.45 mm diagonal
height
> variation at the moment (one corner point to the sky and one down to the
> earth). Any remedy for the "cure"at this stage? ? (it is Au/Ni plated).
> Anything I can do to prevent from happening besides specify the annealed
Cu
> must be used? (can't reflow on the other side, it has to bond to fan by
> thermal compound). Never see anything like that. The internal residual
> stress must be extremely high!
> Thanks in advance for all your help...;-(
> jk
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|