Hi All,
I have problem using the Kester 955 flux with R245 wire.
We manually used these material to solder a row of connectors.
In term of soldering quality, it is alright, except it turned
white after 3 to 4 days.
Is there anyone has experience such issue, and what can I do
to prevent this from happening.
Our customer is not very happy with the white stuffs, but
there is not solution to the issue.
Thanks.
Poh
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------