TECHNET Archives

June 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 21 Jun 2002 12:40:36 +0300
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, b_ellis <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii
From:
Parts/Attachments:
text/plain (49 lines)
And don't forget that incoming components, including the printed circuit
boards, may be delivered neatly contaminated. If you want hi-rel with
"no-clean" chemistry, all you may be doing is, instead of having one
cleaning operation, you may have displaced it to each of your suppliers.
Furthermore, you need to do much more process control and in-house
qualification testing. Be careful that it does not cost more, in the
long run, than using an easily cleaned chemistry and good cleaning, with
easier soldering as a side-benefit.

Brian

> Bogert wrote:
>
> 6/20/2002
>
> Folks is anyone manufacturing military PWAs using no-clean flux and
> not cleaning the PWAs prior to shipment?  If so, what is your
> reliability experience with this process?
>
> We are considering a military application (Class 2) where mixed
> technology (SMT and PTH) PWAs will be soldered using no-clean flux and
> then not conformal coated (assuming the uncoated PWAs can pass our
> temperature/humidity qualification testing).  Although the no-clean
> flux we will use should be benign (we are having SIR testing performed
> to confirm this and Omegameter testing), I am concerned that
> contamination may be introduced by other shop processes such as
> mechanical assembly, testing, etc., even if one uses gloves or fingere
> cots during handling.  One could argue that after shipment, since the
> PWAs are not conformal coated, you can introduce contamination in the
> field and therefore, why not not clean prior to shipment.
>
> We may be performing board testing (boundry scan, bed-of-nails, etc)
> on PWAs that have been soldered using no-clean flux.  I understand
> that certain noclean flux can impede this testing, and also, may cause
> problems in event we need to conformal coat the PWAs.
>
> Any comments on this subject will be appreciated.

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2