TECHNET Archives

June 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 21 Jun 2002 06:30:14 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Content-type:
text/plain; charset=iso-8859-1
Subject:
MIME-Version:
1.0
Content-transfer-encoding:
quoted-printable
From:
"Gordon F. Davis Jr" <[log in to unmask]>
Parts/Attachments:
text/plain (76 lines)
May I get an e-copy of the paper you refered to as well.  I also work for a
military supplier, but we clean everything.  I would like to get further
info on no-clean.

Gordon Davis
Application Engineer
Rockwell Collins




David Douthit <[log in to unmask]>@ipc.org> on 06/20/2002 09:10:13 PM

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
       to David Douthit <[log in to unmask]>

Sent by:    TechNet <[log in to unmask]>


To:    [log in to unmask]
cc:

Subject:    Re: [TN] Cleaning of Military PWAs That Have Been Soldered
       withNo-CleanFlux


You have landed in a very nasty area. You are correct to be concerned about
contamination issues.
Even if the residues from the flux do not create migration/leakage current
problems they may
collect other airborne contaminates that can cause problems.

Process, shipping, and storage control are critical to the reliability  of
the circuitry.

If you wish I have a paper I presented in May of 2001 titled
"Avionics Systems, Reliability, and Harsh Environments"
that I could e-mail you. The information in the paper will
give you a good idea of what type of airborne contamination
issues you may have to deal with.

David A. Douthit
Manager
LoCan LLC

Bogert wrote: 6/20/2002 Folks is anyone manufacturing military PWAs using
no-clean flux and not cleaning the PWAs prior to shipment?  If so, what is
your reliability experience with this process? We are considering a
military application (Class 2) where mixed technology (SMT and PTH) PWAs
will be soldered using no-clean flux and then not conformal coated
(assuming the uncoated PWAs can pass our temperature/humidity qualification
testing).  Although the no-clean flux we will use should be benign (we are
having SIR testing performed to confirm this and Omegameter testing), I am
concerned that contamination may be introduced by other shop processes such
as mechanical assembly, testing, etc., even if one uses gloves or fingere
cots during handling.  One could argue that after shipment, since the PWAs
are not conformal coated, you can introduce contamination in the field and
therefore, why not not clean prior to shipment. We may be performing board
testing (boundry scan, bed-of-nails, etc) on PWAs that have been soldered
using no-clean flux.  I understand that certain noclean flux can impede
this testing, and also, may cause problems in event we need to conformal
coat the PWAs. Any comments on this subject will be appreciated.



---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2