IPC-A-610C section 9.1.3 mentioned the following coating thickness :
Type AR Acrylic resin    0.03 - 0.13mm
Type ER Epoxy resin    0.03 - 0.13mm
Type UR Urethane resin    0.03 - 0.13mm
Type SR Silicon resin    0.05 - 0.21mm
Type XY Paraxlyene resin    0.01 - 0.05mm

Questions asked on behalf of my colleague are :
1. How does one arrive at the coating thickness for each types of
coating material?
2. What is the impact to my board or components if my coating thickness
exceed or below the range stated above?

Regards - Wee Mei

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2