Hi Korringa,
We have an Ersa 500 to replace BGA's, we clean the pads on the PCB with
solder wick then apply a no clean tack flux ( Interflux), via syringe. Then
place the BGA and reflow with excellent results.
Hope this helps.
Steve.
Prod Eng.
-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: 14 May 2002 15:34
To: [log in to unmask]
Subject: [TN] BGA replacement
The M.E.s at my company are struggling with replacing a defective plastic
BGA.
We have an Air Vac BGA machine. The lead M.E. feels that he needs a solder
pad
deposit in place before putting the replacement BGA on the board for reflow.
He
feels that he will compensate for irregular solder balls on the part and
also
possible surface differences on the existing pads which have been wicked
clean
of solder.
The problem is in putting down the paste. He is teaching a technician to use
a
small medium stiff plastic stencil. The paste is applied with a wide chisel
blade x-acto knife looking tool. They are getting uneven solder cakes and
icicles between the solder deposits.
I ask, is that the best way to put down paste? Is it necessary on a plastic
BGA
to put down a paste deposit? Will the stringers pull in when heated or will
they
results in shorts after reflow?
Any info appreciated.
Thanks,
Stu Korringa
Quality Engineer
Smiths Industries Electronic Systems
Grand Rapids, Mi.
**********************************************************************
This e-mail and any files transmitted with it are confidential and may
be legally privileged or otherwise exempt from disclosure under
applicable law. This e-mail and its files are intended solely for
the individual or entity to whom they are addressed and their content
is the property of Smiths Aerospace. If you are not the intended
recipient, please do not read, copy, use or disclose this communication.
If you have received this e-mail in error please notify the e-mail
administrator at [log in to unmask] and then delete this e-mail, its
files and any copies.
This footnote also confirms that this e-mail message has been scanned
for the presence of known computer viruses.
***********************************************************************
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
________________________________________________________________________
This e-mail has been scanned for all viruses by Star Internet. The
service is powered by MessageLabs. For more information on a proactive
anti-virus service working around the clock, around the globe, visit:
http://www.star.net.uk
________________________________________________________________________
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|