Dick,
We are using a connector that you describe, two rows of 5 pins. We use a
8mil stencil cut 1:1 and it solders fine. IPC does not give a whole lot of
detail as to how much solder fillet or anything, just that the fillet
length along the side be a minimum of the width of the pin (25mils), we get
that easy. The heal fillet is were you will run into problems. (as you
stated). Our design guys made a note on the drawing to eliminate
confusion, but we come pretty close to meeting IPC. We are Class 2 thought.
Good luck
David
Ascom Energy
Palm Coast, FL
"Krug, Dick" <[log in to unmask]>@IPC.ORG> on 05/03/2002 10:04:51 AM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to "Krug, Dick" <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: [TN] Class 3 Solder Fillets - SMT 25 mil square pin Headers?
We assemble primarily IPC class 3 products. We have now got some SMT
headers, using 25 mil square pins bent to form a "gull wing" style lead.
There is no way we can get a solder fillet to reach a 25 mil thick lead
thickness. Can these be assembled to meet Class 3 requirements? I think
I've seen something indicating a deviation from these requirements, but I
don't know where nor can I find it again. Any suggestions?
Dick Krug
Sypris Electronics
Tampa, FL
[log in to unmask]
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|