Dave,
I wish I could tell you all the expericnces I've had. It's a long list but
starting from the bent column situation, they are a problem both in
production and rework.
Please be advised these devices had cast columns not clasp. Also, the use
environment was strictly commercial as in Cray and SGI products. Cray had
much higher quality and reliability requirements than SGI even though SGI
used to own Cray.
I started doing this stuff, along with my very good associates, about three
years ago. Under "normal" use conditions, these things are still working
today - according to those same associates with whom I maintain close
contact.
Only concern I really had was the very large physical mass sitting on all
those little columns. No matter, at a 1200 column count, they were well
supported.
Just know the comumns are very compliant, even to the point of being bent.
Does require some careful inspection and straightening, if needed, before
placement and soldering.
Just don't know how these things work under your operational conditions.
Sure would like to know but I like them over BGA's any day for normal stuff.
Also need to add here: No mechanical stress or shock but considerable
thermal stress during operation. Used some exoctic cooling at times but not
always.
Earl
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|