I don't know about other people, but if you read the soldering information
of IBM for ceramic BGA, you will find it there, reccommended for CGA too.
From what I heard, it is not so good for columns- I suppose that this is
because placement has to be done with applied force and maybe if the
columns are nor perfectly aligned or the device is nor at 90*, they will
deform, causing shorts or break. We forgot to apply force the first time
(SRT has the option) and The results were not good, Don't forget that the
stencil is upside down and the bulk of paste is on the balls, with less
paste towards the circuit. Also, the stencilreccomendations are special,
balls with the same pitch but different dimensions get more or less paste
volume, as more or less of the ball is intruding the aperture.
Gaby
----- Original Message -----
From: "Earl Moon" <[log in to unmask]>
To: <[log in to unmask]>; <[log in to unmask]>
Sent: Friday, May 31, 2002 6:47 PM
Subject: Re: NTC - The Gregory's are a team now...
> I'm with you Gaby,
>
> Got to get the pumpkin shape when the balls squat. Very even ball shapes
in
> Xray verify this clearly as well as edge visualization. You know all this
> stuff so I wish you well and keep us all informed about the Genrad gizmo.
I
> like it. Has anyone else tried it, I wonder?
>
> Earl
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|