Bill,
I agree with you almost 100%. I say almost because there is one application we have that must be soldered before crimping, Litz wire. This has many fine strands each with an enamel coating. To remove the coating we dip solder the wire ends in a solder pot. We have tried the enamel strippers in the past, but found them unsatisfactory so we solder and then crimp these wires. Now If I can convince my engineers that you are right for all other applications life will be wonderful... well, better anyway.
Phil Nutting
-----Original Message-----
From: Kasprzak, Bill (sys) USX [mailto:[log in to unmask]]
Sent: Friday, May 17, 2002 7:32 AM
To: [log in to unmask]
Subject: Re: [TN] Crimped connections
Stu,
I've read all of the responses so far but think they all miss the mark. A
crimped connection is designed to "rearrange", for lack of a better word,
the strands of wire within a conductor. This "rearrangement" is created when
a crimp tool compresses the barrel of the lug so that the internal strands
can conform to this compression without breaking the strands. That's why
some crimp tools have different settings for different gauge wire. I've seen
video of crimped connections where this attachment methodology is actually
stronger than soldering the wire to the same lug. Therefore, tinning a wire
before crimping defeats the design of what crimping is supposed to do. We
crimp wires on a regular basis. We perform pull testing on crimped
connections and typically the wire breaks before the crimp pulls out of the
pin. Can't get any stronger than that! So, never tin a wire before crimping,
again never! However, would I rework the lugs that you have? Assuming
something less than class 3, probably not, but it would be the last time I'd
allow it
Bill Kasprzak
Moog Inc. Manufacturing Engineering, Electronics
> -----Original Message-----
> From: [log in to unmask] [SMTP:[log in to unmask]]
> Sent: Thursday, May 16, 2002 7:46 AM
> To: [log in to unmask]
> Subject: [TN] Crimped connections
>
> All-knowing TechNet,
>
> Yesterday I rejected some assemblies that had wires crimped into lugs and
> attached to a TO-3 case. The inspector had noticed that the wires were
> also
> tinned and then had been crimped. I said to rework based on the knowledge
> that
> we had never tinned wires to be crimped.
>
> But when pressed for the reasons behind my decision, I was stumbling for
> an
> answer. All I could come up with is that perhaps the crimp would be less
> crimplified (new word) over time due to solder creep or temperature
> excursions
> since the solder might reflow to some degree.
>
> What is the reason or doesn't it really matter whether tinned or not?
>
> Did this Quality lug crimp his position as the local answer man?
>
> Thanks to the forum,
>
> Stu Korringa
> Quality Engineer
> Smiths Industries Electronic Systems
> Grand Rapids, Mi.
>
>
> **********************************************************************
> This e-mail and any files transmitted with it are confidential and may
> be legally privileged or otherwise exempt from disclosure under
> applicable law. This e-mail and its files are intended solely for
> the individual or entity to whom they are addressed and their content
> is the property of Smiths Aerospace. If you are not the intended
> recipient, please do not read, copy, use or disclose this communication.
> If you have received this e-mail in error please notify the e-mail
> administrator at [log in to unmask] and then delete this e-mail, its
> files and any copies.
>
> This footnote also confirms that this e-mail message has been scanned
> for the presence of known computer viruses.
> ***********************************************************************
>
> --------------------------------------------------------------------------
> -------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
> SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
> -------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|