I may be out of date, Guy, or maybe there's a deficiency in IPC-A-610, but
in the MIL Spec days, the law in my previous company was "there shall be no
exposed copper", and the assembly process had the Wave Solder - Trim Leads
- 2nd Wave Solder operations built into the Master Assembly Instruction
documents (before the solder joint damage with this sequence was
recognised).
If exposed copper is now acceptable, what changed (class 3 boards I'm
talking about)? Part of the reason for over-soldering exposed copper was to
prevent the copper oxidising, and part of the reason was to prevent cut
leads puncturing the conformal coating. Any modern info gratefully
received.
Peter
"Guy Ramsey" <[log in to unmask]> 03/05/2002 07:10 PM
To: "TechNet E-Mail Forum." <[log in to unmask]>, DUNCAN
Peter/Asst Prin Engr/ST Aero/ST Group@ST Domain
cc:
Subject: RE: [TN] Wave solder re-runs/re-work exposed
copper
I agree with you, as far as trimming leads before soldering. I agree, a
solder - cut - solder process should be avoided if possible.
But, I can't find any place in the J-STD-001C or IPC-A-610C which bans
exposed copper. In fact, I can only find places where it is specifically
acceptable, even including nicked leads unless the damage is greater than
10% of the lead diameter or thickness. Unless the damage is the result of
careless or repeated bending.
Is this a topic worthy of discussion? Have I misinterpreted the standards?
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of
> [log in to unmask]
> Sent: Thursday, May 02, 2002 8:05 PM
> To: [log in to unmask]
> Subject: Re: [TN] Wave solder re-runs/re-work
>
>
> One thing I've learned in my 20+ years in electronics
> manufacturing is that
> one should pre-trim leads prior to soldering, not trim them afterwards,
> especially with the plier type lead cutters. The shock to the solder
> joints when the leads part with that snap is very high, and joints, too
> numerous to mention, have been damaged in the process. Even
> high-speed lead
> saws aren't much better, and often tend to smear leads rather than cut
> them. I've also known these cut right through a joint and into a
> board when
> the board is a bit bowed (bowed boards weren't so critical back then with
> plated-through-hole components).
>
> Also, on class 3 boards anyway, exposed copper is banned, so all trimmed
> leads had to be put back through the wave solder to cover them up. This
is
> an additonal and unnecessary thermal excursion that should be
> avoided. It's
> detrimental to the life of the board and takes extra time and cost for
the
> additional processes involved. It's better to trim the leads to length
> prior to soldering then wave solder only once. Clinch or half-clinch two
> opposing leads on each component before trimming if you're worried about
> the components rising in the wave, or put a pad over the
> components to hold
> them in place.
>
> One holding technique I saw years ago is to vacuum-form thin plastic
sheet
> over the populated board that can be peeled or lifted off after the
> soldering process. We never tried it, and I never saw it used "for real",
> so I don't think it caught on. Another technique was to secure a foam pad
> over the components (wave resistant, of course)
>
> Anyway, in your current curcumstances, I would opt for doing a second
wave
> solder pass, in spite of what I just said, especially if you have a lot
of
> leads to do on a lot of boards. It will be kinder to the board
> that locally
> heating lots of areas, though your no-clean residues will build up. Maybe
> our TN cleaning experts can help with that one.
>
> Good luck
>
> Peter
>
>
>
> David White <[log in to unmask]> 02/05/2002 11:14 PM
> Sent by: TechNet <[log in to unmask]>
>
> Please respond to "TechNet E-Mail Forum."; Please respond to David White
>
> To: [log in to unmask]
> cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group)
> Subject: [TN] Wave solder re-runs/re-work
>
>
>
>
>
>
>
>
> Advice please. We have had a problem here we have cut in the
> solder fillet
> while trimming leads (pretty deeply, we have also seen cracked solder
> fillets) which is a violation of IPC. There are several hundred of these
> asm. I suggested to Re-run them through wave. Has anyone else had to do
> this and what have the results been, this sure beats touch-up on every
> lead. I am not re-fluxing the asm, we spray no-clean and some
> gets on the
> top the 1st time around which is acceptable, but 2nd time it is just to
> much. Anyone have any comments? Any help would be great.
> Dave
>
> ------------------------------------------------------------------
> ---------------
>
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
> SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> ------------------------------------------------------------------
> ---------------
>
>
>
>
>
> [This e-mail is confidential and may also be privileged. If you
> are not the
> intended recipient, please delete it and notify us immediately; you
should
> not copy or use it for any purpose, nor disclose its contents to any
other
> person. Thank you.]
>
> ------------------------------------------------------------------
> ---------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ------------------------------------------------------------------
> ---------------
>
[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|