Unbelievable.
Just last month, you may recall, we discussed warping in a particular type
of BGA package. A TechNet subscriber gave me a POC at the semi-conductor
manufacturer (not listed as subscribing to the NEDA paper). The very first
thing the package designer asked for was the country and date codes. Given
those to data points the semiconductor manufacturer was able to identify the
materials and processes used to create the package, the root cause of the
OEM problems and suggest corrective action.
The components inside the bag undoubtedly were marked but can you imagine if
the components in these bags were of mixed origin and/or date of
manufacture.
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of [log in to unmask]
> Sent: Tuesday, April 30, 2002 11:14 PM
> To: [log in to unmask]
> Subject: [TN] A "NEDA" Oriented label...
>
>
> Was given a image of a label on packaging that's out there as we speak, as
> something that would be more wide-spread if NEDA has their way...go to:
>
> http://www.stevezeva.homestead.com
>
> and look at NEDA label.jpg...
>
> Really helps, doesn't it?
>
> -Steve Gregory-
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|