Well, yes!
As I said in my earlier postings, there have been some developments that
make this whole exercise easier / cheaper (sorry - less expensive) and
more convenient than the "good old days"!
I fully take on board your comment Earl, about equipment support. That
is an issue as it always was with relatively new "start-up's". However,
we can all get there in the end and can / have learned from the past....
If anyone is keen / willing / able, I will be happy to negotiate a demo
system to a suitable location that everyone can then critique. Earl,
Steve, you seem like suitable candidates for criticism of a new
technology, how about it? It can't be free, cos I ain't made of money -
contrary to the views of some!
Regards Graham Naisbitt
[log in to unmask] <mailto:[log in to unmask]>
Concoat ANNOUNCE their acquisition of the former Multicore SPCID
business.
MUST II Solderability Testing Systems -
CM Cleanliness Testing Systems -
Auto-SIR Reliability Testing Systems -
SoldaPro & NEW SoldaPro Wizard Thermal Profilers
For more information please visit our new web site:
www.concoatsystems.com <http://www.concoatsystems.com>
Concoat Limited
Alasan House, Albany Park
Camberley GU16 7PH - UK
www.concoat.co.uk <http://www.concoat.co.uk>
Phone: +44 1276 691100
Fax: +44 1276 691227
Mobile: +44 79 6858 2121
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Earl Moon
> Sent: Tuesday, May 28, 2002 21:06
> To: [log in to unmask]
> Subject: Re: [TN] Vapor phase
>
>
> Right on Steve,
>
> Always great to know someone who's been there and done that.
> Lot's of folks out there now reinventing the wheel that first
> was turned in the late '70's with the first military SMT
> stuff then on to trillium like stuff in the early to mid '80's.
>
> Outstanding, and I really want to know more about the latest
> condensation reflow technology. Anything new Mr. Nasbitt?
>
> Earl
>
> --------------------------------------------------------------
> -------------------
> Technet Mail List provided as a free service by IPC using
> LISTSERV 1.8d To unsubscribe, send a message to
> [log in to unmask] with following text in the BODY (NOT the
> subject field): SIGNOFF Technet To temporarily halt delivery
> of Technet send e-mail to [log in to unmask]: SET Technet
> NOMAIL To receive ONE mailing per day of all the posts: send
> e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at:
> http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/html/forum.htm for additional information, or contact
Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
------------------------------------------------------------------------
---------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|