Steve,
When you say "massive failures", are you talking electrical or just the
delamination problem?
Some of our military products use PPS caps, and we see delamination after
going through water wash. There are many layers of the plastic film to
protect the dielectric layers underneath. We had similar concerns about
the delam so we have run 2000 temperature cycles, from -54C to +125C on 200
of various package sizes of these parts with 50% of the rated voltage
applied, postcoated and unpostcoated, without any failures or increase in
leakage current. We have since allowed for delamination of these parts in
our component specification.
These are great capacitors electrically, that can have higher capacitance
values without the leakage issues of ceramic caps.
Jim Carlson
Rockwell Collins Reliability Engineer
[log in to unmask]@ipc.org> on 05/23/2002 08:51:58 PM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to [log in to unmask]
Sent by: TechNet <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: [TN] Film Capacitors...geeze!
Hi all!
Just started building an assembly that calls out film capacitors to be used
in 64-locations on the board. Processed the assemblies in a typical manner
as
one would for most SMT assemblies, and experienced massive failures of
these
caps. They are PPS films. Unfortunately, this has been a first for
me...never
had to process these caps before. They are delaminating...the layers of
film
are flaking off from the caps.
Can anybody tell me how I should assemble these devils? Went to the web
page
of the manufacturer, and they have a recommended reflow profile that is
2-mins, 45-seconds long...to me, that violates the specifactions that
Kester
recommends for their paste to perform...
Is using SMT film caps a bad idea? ( I think I know the answer, but I just
want a confirming opinion...)
-Steve Gregory-
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|