TECHNET Archives

May 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Tom Buschor <[log in to unmask]>
Date:
Wed, 22 May 2002 12:13:23 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Tom Buschor <[log in to unmask]>
Parts/Attachments:
text/plain (26 lines)
Steve,

We are using a Loctite material for underfill of BGAs. It does
significantly improve interconnect reliability in thermal cycling and
vibration.

It is reworkable, and we have proven that reworked BGAs are just as
reliable.

On the down-side, rework is time consuming and it has to be done very
carefully to prevent damage to the PWB. A well controlled process is
essential.

Tom

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2