TECHNET Archives

May 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
Frank Kimmey <[log in to unmask]>
Date:
Tue, 21 May 2002 08:25:32 -0700
MIME-Version:
1.0
X-To:
Guy Ramsey <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Frank Kimmey <[log in to unmask]>
Parts/Attachments:
text/plain (97 lines)
Guy,
These are micro8 and sop packages, 25 mil pitch.
Leads may be up to 18 mils wide, while land is only 13 mils (nominal lead
width).

All I have found so far are requirements that do not say a side fillet is
req'd. I would like to find a standard that states a side fillet is not
required.

Thanks for the help,
FNK

Hey Steve,
If you are watching, what is your take on side fillets?
How do you interpret IPC-610 figure 12-71?

Earl,
comments?

Werner,
What loss in integrity and/or reliability is caused by no side fillet?

Thanks to Peter and Gary for your replies, they are reinforcing my case.

Frank N Kimmey, C.I.D.+
Senior PCB Designer
Powerwave Technologies
PH. 916-941-3159
Fax 916-941-3195


-----Original Message-----
From: Guy Ramsey [mailto:[log in to unmask]]
Sent: Tuesday, May 21, 2002 5:58 AM
To: [log in to unmask]
Subject: Re: [TN] Side fillet requirements


Something is wrong. What type of component are we discussing? Side joint
requirments are specific to component types.

If there is a compliant land pattern that is narrower than the lead width it
would be new to me.

I have seen "compliant design" reduced by undercut resulting land patterns
like you describe.

> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Frank Kimmey
> Sent: Monday, May 20, 2002 6:17 PM
> To: [log in to unmask]
> Subject: [TN] Side fillet requirements
>
>
> I have a customer who would like us to justify why our IPC-782 compliant
> footprints do not allow for a side fillet (pad width is equal to
> or smaller
> than lead width). I did not find conclusive statement in IPC-610
> concerning
> this. Please help me define acceptance.
>
> Thanks,
> FNK
>
> Frank N Kimmey, C.I.D.+
> Senior PCB Designer
> Powerwave Technologies
> PH. 916-941-3159
> Fax 916-941-3195

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2