No side fillets are usually found on fine-pitch QFP's and the like, where
really there isn't the room to have pads wider than the leads without an
attendant risk of solder bridging. If you have a class 2 product, side
fillets aren't an issue. For class 3, we have to grin and bear it. Toe and
Heel fillets are the important fellows when considering solder joint
strength.
Peter
Frank Kimmey <[log in to unmask]> 21/05/2002 06:16 AM
Sent by: TechNet <[log in to unmask]>
Please respond to "TechNet E-Mail Forum."; Please respond to Frank Kimmey
To: [log in to unmask]
cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group)
Subject: [TN] Side fillet requirements
I have a customer who would like us to justify why our IPC-782 compliant
footprints do not allow for a side fillet (pad width is equal to or smaller
than lead width). I did not find conclusive statement in IPC-610 concerning
this. Please help me define acceptance.
Thanks,
FNK
Frank N Kimmey, C.I.D.+
Senior PCB Designer
Powerwave Technologies
PH. 916-941-3159
Fax 916-941-3195
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|