TECHNET Archives

May 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-type:
text/plain; charset="us-ascii"
Sender:
Subject:
From:
Date:
Thu, 16 May 2002 08:02:54 -0500
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (23 lines)
Phil,
One suggestion is to look at the amount of resin on the surface of the
board.  Often times, when tracking occurs along the fibers of the
reinforcement, the buttercoat, or the thin layer of resin at the top of the
board that seals off the fibers, is very thin and may expose the glass.  If
so, then the fibers can wick contaminants into the bundles by capillary
action and is impossible to get out.  Tracking then follows those
contaminants.

Doug Pauls
Rockwell Collin

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2