TECHNET Archives

May 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Date:
Thu, 16 May 2002 10:39:09 +0800
Content-type:
text/plain; charset=us-ascii
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (33 lines)
Hello Guys?
Can anybody explain the separation of Solder Bump from UBM after the
Assembly Process?

Solder Bump=95Pb5Sn Alloy
It is plated on a wafer with Under Bump Metal (UBM) of TiCuNi. It then
reflowed to form a bump (And is Fluxed).

The bumped wafer then assembled, after assembly there were weak bumps which
some of them separated from the UBM.
Can you explain this phenomena? would this be intemetallic effects? Is it
possible to have this phenomena that is caused by mechanical vibration plus
the heat applied?
By the way the reflow profile had a peak temp of 285 C.

I can't figure out yet why this happened?
Any inputs would lead me to solve this problem

regards

Jonathan

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2