TECHNET Archives

May 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 10 May 2002 11:25:18 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Content-type:
text/plain; charset=iso-8859-1
Subject:
MIME-Version:
1.0
Content-transfer-encoding:
quoted-printable
From:
Dave Hillman <[log in to unmask]>
Parts/Attachments:
text/plain (49 lines)
Hi Phil! Any issues with soldering to the tin/nickel finish? Is the
assembler using a highly active flux?

Dave Hillman
Rockwell Collins
[log in to unmask]





Phillip Hinton <[log in to unmask]>@ipc.org> on 05/09/2002 11:39:51 AM

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
       to [log in to unmask]

Sent by:    TechNet <[log in to unmask]>


To:    [log in to unmask]
cc:

Subject:    [TN] Ceramic filled Teflon board


All

I had an inquiry as to who could supply a  8 layer multilayer for the
Rogers ceramic filled polytetrafluoroethylene laminate for an RF
application.  My initial calls did not yield a fabricator.

Also the final finish was tin-nickel.  I have not heard of anyone using it
for 20 years.  Does anyone still supply it.

Phil Hinton
520-745-1013


---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2