TECHNET Archives

April 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Andre Leclair <[log in to unmask]>
Date:
Tue, 23 Apr 2002 10:24:39 -0700
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, David Douthit <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii; x-mac-type="54455854"; x-mac-creator="4D4F5353"
From:
David Douthit <[log in to unmask]>
Parts/Attachments:
text/plain (50 lines)
Andre,

If the flux gets in there so will the solder!

David A. Douthit
Manager
LoCan LLC

Andre Leclair wrote:

> We have recently run across a situation which has baffled us.  On the PCB
> in question there are 4 Wave soldered PLCC sockets. 1 of these is being
> reported as having solder shorts underneath.  On the returned units we x-
> rayed the sockets ( can't see under) and found shorts on 1 socket location
> only.  The shorts were consistanly on the same pin area for all the sockets
> were the shorts were found.  We removed a socket only to find the board
> very clean underneath...no shorts..
> The socket has a bottom retainer to hold all the pins in place.. This was
> pried off and to our surprise there was the short.. inside the connector.
> The amount of solder was enough to surround 3 pins in 2 seperate areas.
> The hole around the pins in the plastic base is no more then 0.002".
>
> Does any one have any idea how solder could have gotten up inside the
> connector ( consistantly in the same location)? Or has any one seen this
> before?
>
> We have run this assembly several times in the past with no difficulty.
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2