Andre,
If the flux gets in there so will the solder!
David A. Douthit
Manager
LoCan LLC
Andre Leclair wrote:
> We have recently run across a situation which has baffled us. On the PCB
> in question there are 4 Wave soldered PLCC sockets. 1 of these is being
> reported as having solder shorts underneath. On the returned units we x-
> rayed the sockets ( can't see under) and found shorts on 1 socket location
> only. The shorts were consistanly on the same pin area for all the sockets
> were the shorts were found. We removed a socket only to find the board
> very clean underneath...no shorts..
> The socket has a bottom retainer to hold all the pins in place.. This was
> pried off and to our surprise there was the short.. inside the connector.
> The amount of solder was enough to surround 3 pins in 2 seperate areas.
> The hole around the pins in the plastic base is no more then 0.002".
>
> Does any one have any idea how solder could have gotten up inside the
> connector ( consistantly in the same location)? Or has any one seen this
> before?
>
> We have run this assembly several times in the past with no difficulty.
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|