Any particular flux and conformal coating combo Susan?
We have done some work which showed the choice of resist, flux and
coating were influential in the successful outcome of conformal coating
operations.
We found the results varied quite considerably depending on the
materials choices. Please contact me offline if you think this might be
of interest.
Either way, extensive SIR and thermal cycling/shock testing should be
performed to check the electrochemical reliability of the combination as
well as establishing the impact of the flux residues in reducing the
adhesion of the coating.
Hope of some use,
Best Regards,
Phil Kinner
Chief Chemist
Concoat Ltd
2C Albany Park, Frimley Road,
Camberley, Surrey, GU16 7PH
Tel: +44 (0) 1276 691100
Fax: +44 (0) 1276 691227
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
Sent: 07 February 2002 14:23
To: [log in to unmask]
Subject: Re: [TN] Conformal coat over Low solids flux
Sent this the first time with help as the first word and it got kicked
out.
I have searched the archives for info and have not been successful.
Where can I go to find info on the success of putting conf coat over
low-solids fluxes.
Susan Mansilla
Robisan Lab
------------------------------------------------------------------------
---------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases
> E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
------------------------------------------------------------------------
---------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|