Any particular flux and conformal coating combo Susan? We have done some work which showed the choice of resist, flux and coating were influential in the successful outcome of conformal coating operations. We found the results varied quite considerably depending on the materials choices. Please contact me offline if you think this might be of interest. Either way, extensive SIR and thermal cycling/shock testing should be performed to check the electrochemical reliability of the combination as well as establishing the impact of the flux residues in reducing the adhesion of the coating. Hope of some use, Best Regards, Phil Kinner Chief Chemist Concoat Ltd 2C Albany Park, Frimley Road, Camberley, Surrey, GU16 7PH Tel: +44 (0) 1276 691100 Fax: +44 (0) 1276 691227 -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask] Sent: 07 February 2002 14:23 To: [log in to unmask] Subject: Re: [TN] Conformal coat over Low solids flux Sent this the first time with help as the first word and it got kicked out. I have searched the archives for info and have not been successful. Where can I go to find info on the success of putting conf coat over low-solids fluxes. Susan Mansilla Robisan Lab ------------------------------------------------------------------------ --------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ------------------------------------------------------------------------ --------- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------