IMHO: not much help with agressive OA fluxes.
opens process windows a bit with no-cleans.
may be important for Lead-Free processing.
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Grant Emandien
> Sent: Wednesday, February 06, 2002 10:38 AM
> To: [log in to unmask]
> Subject: [TN] Nitrogen atmosphere reflow soldering: Costs & Benefits
>
>
> 'netters,
>
> I am presently exploring the cost-benefits of nitrogen atmosphere
> soldering
> in our facility. Opinions and recommendations in literature
> obtained thusfar
> has been broad and varied. Some bemoan costs while others hail defects
> reduction. We presently have a nitrogen atmosphere wave soldering facility
> and yes, dross reduction leading to better looking joints.
>
> But what have your experiences been and the benefits gained by using
> nitrogen for (a) no-clean and (b) water-soluble solder?
>
> What are the limitations and any disadvantages of using nitrogen?
>
> TIA
> Grant
>
>
> **********************************************************************
> Notice:
>
> The information contained in this e-mail (including any
> attachments) may contain commercially sensitive or confidential
> information which may be legally privileged and is for the sole
> use of the intended recipient(s). If you are not, or believe you
> may not be, the intended recipient, you are hereby notified that
> any use, dissemination, copying, review, disclosure or action
> taken in reliance of this e-mail is prohibited and may be
> unlawful. If you have received this message in error, please
> notify the sender immediately by reply e-mail and delete all
> copies of the message.
>
> Any views expressed in this message are those of the individual
> sender unless expressly stated by the sender to be given on
> behalf of Tellumat (Pty) Ltd. Tellumat (Pty) Ltd disclaims
> liability for any unauthorised opinion or representation made by
> the sender on behalf of Tellumat (Pty) Ltd.
>
> No warranty is given by Tellumat (Pty) Ltd that the integrity or
> security of this e-mail (including any attachments) has been
> maintained through transmission, nor that the communication is
> free of virus, interception or interference.
>
> **********************************************************************
>
> ------------------------------------------------------------------
> ---------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search previous postings at: www.ipc.org > On-Line Resources &
> Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ------------------------------------------------------------------
> ---------------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|