Hi James,
Start listing all your assumptions regarding materials (parts, solder, flux)
, machines, people (man) training, and the process. What's the same and
what's different between the two setups? You've already clearly stated the
problem - one solder pot is giving you wetting trouble while another isn't.
It doesn't sound like the solder is the culprit since the analysis shows
them to be very similar.
The first time I got called down to solve a solder problem it turned out to
be the flux - 15 years past it's expiration date. RMA flux the color of a
good stout. The new guy on the line couldn't figure out why the boards
weren't soldering.
Hans
Integrity First - Service Before Self - Excellence in All We Do
~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~
Hans M. Hinners
Electronics Engineer
Warner Robins - Air Logistics Center (WR-ALC/LUGE)
226 Cochran Street
Robins AFB GA 31098-1622
mailto:[log in to unmask]
Com: (478) 926 - 5224
Fax: (478) 926 - 4911
DSN Prefix: 468
-----Original Message-----
From: James TerVeen [mailto:[log in to unmask]]
Sent: Thursday, February 07, 2002 4:22 PM
To: [log in to unmask]
Subject: [TN] Solder pot
Forgot to say that we are the manufacturer of Multilayer Chip Capacitors
and we do this operation all the time. We tried solder coating the parts
in both pots using the same flux and got different results
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|