Hi Tom,
I ran into this problem a few years ago - check the list archives. As I
recall, the consensus was the flux core was protected by the solder and
shouldn't expire. A down & dirty test could be to compare basic
solderability for the expired with in date flux-core wire. If the stuff
still wets, passes a pull test and can't be distinguished from in date
solder then you could "requalify" it. I'd be interested to hear what one of
the solder manufacturer's has to say about a requal procedure. It might be
more of a marketing tool, such as the "best used by" date on soda cans.
Hans
Integrity First - Service Before Self - Excellence in All We Do
~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~
Hans M. Hinners
Electronics Engineer
Warner Robins - Air Logistics Center (WR-ALC/LUGE)
226 Cochran Street
Robins AFB GA 31098-1622
mailto:[log in to unmask]
Com: (478) 926 - 5224
Fax: (478) 926 - 4911
DSN Prefix: 468
-----Original Message-----
From: Roger Bilham [mailto:[log in to unmask]]
Sent: Wednesday, February 13, 2002 2:49 AM
To: [log in to unmask]
Subject: Re: [TN] requalification of expired flux-core solder
As a follow-up question, has anyone ever come across flux cored wire
which has become functionally defective through age? Provided that the
temperature isn't excessive and the outer layers of the wire are
protected from surface oxidation, cored wire should last almost
indefinitley, shouldn't it?
Roger Bilham
In article <48359946794DD511BA3A00508BA5563F0ECE1A@MERCURY>, Ochenas,
Tom <[log in to unmask]> writes
>
> Does anyone know of a method/standard for requalifying expired flux
> core solder wire (62/36/2)?
>
> The simpler the better...
>
> Thanks In Advance,
>
> Tom Ochenas
> Process Engineering
> Maxtek Components Corporation
--
Roger Bilham
Roger Bilham Consultancy
Tel: +44 (0)20 8467 8819
Fax: +44 (0)8700 548 613
Mobile +44 (0)7 941 122 446
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|