TECHNET Archives

January 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Kathy Kuhlow <[log in to unmask]>
Date:
Wed, 30 Jan 2002 08:19:46 -0600
Content-Type:
multipart/mixed; boundary="=_08556105.23422F27"
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Kathy Kuhlow <[log in to unmask]>
Parts/Attachments:
text/plain (304 bytes) , TEXT.htm (672 bytes)
IPC-610 has no-clean residues as acceptable.  Is it possible that flux may have been mixed with a washable?  Washing a no-clean off is more detrimental than leaving it alone.  

Is the assembly conformally coated?  Is the application intended to be in a wet or high humidity/moisture enviroment?

Kathy 



<!DOCTYPE HTML PUBLIC "-//W3C//DTD HTML 4.0 Transitional//EN"> <HTML><HEAD> <META http-equiv=Content-Type content="text/html; charset=iso-8859-1"> <META content="MSHTML 6.00.2712.300" name=GENERATOR></HEAD> <BODY style="MARGIN-TOP: 2px; FONT: 10pt MS Sans Serif; MARGIN-LEFT: 2px"> <DIV>IPC-610 has no-clean residues as acceptable.&nbsp; Is it possible that flux may have been mixed with a washable?&nbsp; Washing a no-clean off is more detrimental than leaving it alone.&nbsp; </DIV> <DIV>&nbsp;</DIV> <DIV>Is the assembly conformally coated?&nbsp; Is the application intended to be in a wet or high humidity/moisture enviroment?</DIV> <DIV>&nbsp;</DIV> <DIV>Kathy </DIV></BODY></HTML>