TECHNET Archives

December 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Date:
Mon, 10 Dec 2001 08:40:33 -0000
Reply-To:
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
From:
Mike Fenner <[log in to unmask]>
Parts/Attachments:
text/plain (217 lines)
It's possible that if this correspondence goes on like some of the threads
here quite a few people will end up semi comatose, but perhaps not in the
way you meant:)
Can we also hear if cross linking only takes place by exposure to UV/light
or is initiated by UV/light. And if initiated how is the cure completed?


Best regards

Mike Fenner
Applications Engineer, European Operations
Indium Corporation
 T: + 44 1908 580 400
M: + 44 7810 526 317
 F: + 44 1908 580 411
 E: [log in to unmask]
W: www.indium.com
Leadfree: http://Pb-Free.com



-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Graham Naisbitt
Sent: Sunday, December 09, 2001 7:01 PM
To: [log in to unmask]
Subject: Re: [TN] 2 Conformal Coating ?'s


Peter,

I am semi-comatose now, so please, tell us what exactly are the advantages
of UV curable coatings?

Regards, Graham Naisbitt

[log in to unmask]
www.concoat.co.uk <http://www.concoat.co.uk>

For instant access to Product Data Sheets register on the Tech-Shot area of
http:// www.concoat.co.uk <http://www.concoat.co.uk>

Concoat Limited
Alasan House, Albany Park
CAMBERLEY GU16 7PH UK
Phone: +44 (0)1276 691100
Fax: +44 (0)1276 691227
Mobile: +44 (0)79 6858 2121


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Peter Swanson
Sent: Friday, December 07, 2001 05:51
To: [log in to unmask]
Subject: Re: [TN] 2 Conformal Coating ?'s


Graham,

You really must see someone about your delusions over UV cured coatings,
which are successfully used to coat many thousands of pcb's each year. I
know someone who has a nice sofa you can stretch out on whilst you tell him
all about it.... <g>

Suitability for UV has nothing to do with 3D v. 2D, more to do with the
complexity of the assembly geometry and the application methodology. These
will determine if a secondary cure mechanism is needed for the application.
In many instances (and with some of our customers), full cure is achieved
just with light.

Regards,
Peter
--
--------------------------------------------------------
Peter Swanson        [log in to unmask]
INTERTRONICS            http://www.intertronics.co.uk

   INTERTRONICS is dedicated to providing quality
  material, consumable and equipment solutions to the
 electronics manufacturing and other technology based
  industries, with the highest levels of technical
           support and customer service.


-----Original Message-----
From: Graham Naisbitt [mailto:[log in to unmask]]
Sent: 06 December 2001 16:52
To: [log in to unmask]
Subject: Re: [TN] 2 Conformal Coating ?'s


Mike

You would be better to go with a conventional coating. UV is not ideal for
3D objects - works great in 2D, cos you don't have to bend light! :-)

I cannot remember what the operating environment was for your circuit - if
you would care to repeat, I can recommend something - however, I am sure
that a one part AR or UR coating from a reliable supplier will give you the
best overall results - process and operating environment.

Regards, Graham Naisbitt

[log in to unmask]
www.concoat.co.uk <http://www.concoat.co.uk>

For instant access to Product Data Sheets register on the Tech-Shot area of
http:// www.concoat.co.uk <http://www.concoat.co.uk>

Concoat Limited
Alasan House, Albany Park
CAMBERLEY GU16 7PH UK
Phone: +44 (0)1276 691100
Fax: +44 (0)1276 691227
Mobile: +44 (0)79 6858 2121





-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Mike Manwell
Sent: Thursday, December 06, 2001 02:41
To: [log in to unmask]
Subject: [TN] 2 Conformal Coating ?'s


Hello,
Thanks in advance if you have taken the time to read this!

#1- Im trying different materials in a spray application. Both are cured
using UV. One material does a "secondary cure" w/ moisture. This is cool
because after 100 hours after UV cure, all material is fully cured.
The other material Im trying uses HEAT for a secondary cure, or, if
shodowed during UV cure, the material wont cure and never will. Obviously I
dont want the stuff dripping or running anywhere, but being new to this
wonderful process, just dont feel good about leaving uncured material on a
product for it's entire life. Iv been told that you can "test" the product
to see if the uncured material is causing a problem but Im not sure what
type of test that would consist of. Any insight?

#2- Has anyone out there ever installed refelctive metal plates in their UV
oven to limit shadowing?

Thanks so much,

Mike Manwell

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2