Bob,
I have had good results with Teflon and I-PVC insulated wires in a
reflow application. We even wave soldered a few applications. (sub-merged)
Through testing I found we could a use pin-in-paste method and the
insulation held up well. If you are doing a Pb-free reflow, there may be
issues, as the temps are higher than SnPb.
Do some testing, with TC's attached to the wires. You may be
surprised to see the results.
Good Luck,
Rich
Richard Elensky
Sr. Manufacturing Engineer
[log in to unmask] <mailto:[log in to unmask]>
Tel: 559-292-1111 x246
Fax: 559-292-9355
Dantel
2991 North Argyle Ave.
Fresno, CA, 93727
Visit our web site at:
http:// www.dantel.com <http://www.dantel.com>
----------
From: Bob Donaldson [SMTP:[log in to unmask]]
Sent: Friday, November 16, 2001 8:03 AM
To: [log in to unmask]
Subject: [TN] Soldering wires to PWB with SMT Reflow process
To All,
We have a application where it would be very nice to solder two
small wires
to a PWB assembly while we are reflow soldering the other SMT parts
to the
board. So far we have not found a wire type that a manufacturer will
ensure
will survive the reflow temperatures. Solid wire with insulation is
needed
in the 22-24 awg. size. Does anybody have experience soldering wires
to
assemblies in reflow processes?
Any leads would be appreciated.
Thanks,
Bob Donaldson
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following
text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message:
SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|