Peter and others
You should be aware that there are new developments in coating materials
that render your set-up much simpler and less expensive. These are water
based coatings, VOC free and MIL-Spec qualified. They are repairable and
fast to cure - <30 minutes at room temp.
Dave Fish (hello Dave) gave you the correct info regarding various issues
when dealing with conventional solvent based coatings. However, with these
new water based materials: there are no special fire precautions - the fume
extraction isn't mandatory - your insurance costs will diminish,
significantly - the health & safety of your operators is improved.
If you or anyone else wants more details contact me of-line.
Regards, Graham Naisbitt
[log in to unmask]
www.concoat.co.uk <http://www.concoat.co.uk>
For instant access to Product Data Sheets register on the Tech-Shot area of
http:// www.concoat.co.uk <http://www.concoat.co.uk>
Concoat Limited
Alasan House, Albany Park
CAMBERLEY GU16 7PH UK
Phone: +44 (0)1276 691100
Fax: +44 (0)1276 691227
Mobile: +44 (0)79 6858 2121
Attention: This message is for the named person's use only. It may contain
confidential, proprietary or legally privileged information. No
confidentiality or privilege is waived or lost by any mistransmission. If
you receive this message in error, please immediately delete it and all
copies of it from your system, destroy any hard copies of it securely and
notify the sender. You must not, directly or indirectly, use, disclose,
distribute, print, or copy any part of this message if you are not the
intended recipient. Concoat Ltd and any of its subsidiaries each reserve the
right to monitor all e-mail communications through its networks.
Any views expressed in this message are those of the individual sender,
except where the message states otherwise and the sender is authorised to
state them to be the views of Concoat Ltd or one of its subsidiaries.
Although this message has been scanned for known viruses and inappropriate
content, we recommend that recipients employ appropriate measures on their
systems to intercept any such material.
Thank You - Concoat Ltd
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of peter lee
Sent: Friday, September 28, 2001 04:57
To: [log in to unmask]
Subject: [TN] Setting up conformal coating process
Hello,
I like to hear your thoughts or experiences on setting
up a safe and efficient (in particular exhaust,
floorinconformal coating process g, ESD concerns,
layout, material storage). Please comment on anything
you feel critical to process control and success.
Peter
__________________________________________________
Do You Yahoo!?
Listen to your Yahoo! Mail messages from any phone.
http://phone.yahoo.com
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|