I'm seeing this the same way as Kathy Kuhlow. But, if this board has heavy
internal layers and is preheated enough to get good top side solder fillets,
the solder may still be molten when it comes out of the end of the machine.
Are we looking at disturbed joints here?
Guy Ramsey
Senior Lab Technician / Instructor
E-Mail: [log in to unmask] <mailto:[log in to unmask]>
Ph: (610) 362-1200 x107
Fax: (610) 362-1290
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Kathy Bergman
Sent: Friday, August 10, 2001 2:00 PM
To: [log in to unmask]
Subject: [TN] Solder conditions
I am looking to get some help in identifying the causes of certain post wave
solder conditions. In particular, a "cracked ice" effect in which the very
surface of the solder looks like a thin layer of it has been cracked in the
way that ice would crack. Another one is lumpy solder, as if the solder had
dirt in it. (I know it doesn't). I am a board manufacturer with just a
minimum of assembly knowledge.
I am unable to post a good picture of the conditions at this time. I
am wondering if there are some on line resources I can tap into, to see some
visual examples of these and other conditions.
Also, what would be a normal wave profile for a board such as this: .093
thick FR4, through hole technology, approx. 6x11, .025 to .195 sized holes,
HASL finish. Please include any prebake information.
I apprectiate in advance any help I can get.
Kathy Bergman
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|