TECHNET Archives

October 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Steve Abrahamson <[log in to unmask]>
Date:
Fri, 26 Oct 2001 16:15:53 -0600
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Parts/Attachments:
text/plain (175 lines)
Gents,

If you are using a SmartSonic Ultrasonic cleaner, their technical people say
that because they alternate their ultrasonic frequency, damage to die bonds
should not occur.
You might want to give your Ultrasonic cleaner representitive a call to find
out more specifics.

Steve A

> -----Original Message-----
> From: Guy Ramsey [SMTP:[log in to unmask]]
> Sent: Friday,October 26,2001 12:15 PM
> To:   [log in to unmask]
> Subject:      Re: [TN] Cleaning paste when misaligned.
>
> I don't mean to cause any undue concern. The issue is fairly simple . . .
> You can break glass and ceramic with sound but it is not likely if you are
> careful. But ultrasonic cleaning can break wire bonds, and wires, this is
> especially true in controls, ceramic ICs and the like were the wires are
> not encapsulated and subject to vibration. There are technologies that are
> effective in reducing this type of damage. Hope this relieves your fear.
> If you are still concerned then you have some homework to do. What
> frequency and power does you cleaner work at. What is a construction of
> the packages in question . . . stuff like that.
>
>       -----Original Message-----
>       From: TechNet [mailto:[log in to unmask]]On Behalf Of Howard Watson
>       Sent: Friday, October 26, 2001 11:46 AM
>       To: [log in to unmask]
>       Subject: Re: [TN] Cleaning paste when misaligned.
>
>
>
>       Mike and Guy,
>
>       We routinely clean the second side of misprint solder paste, but
> from what you are saying perhaps there could be a problem with damaging
> some components.  The components that we clean in the ultrasonic cleaner
> are mostly flat chip package, C lead diodes, and some SOT-23 and SOIC.
> How do I verify which components can or cannot go in the cleaner?  Is
> there any test data out there to support this issue?  Though we clean very
> few misprints, I am a little concerned.  Thanks for your help!
>
>       Howard Watson
>       Manufacturing Engineer
>       AMETEK/Dixson
>
>
>
>       "Barmuta, Mike" <[log in to unmask]>
> Sent by: TechNet <[log in to unmask]>
>
> 10/26/01 09:02 AM
> Please respond to "TechNet E-Mail Forum."
>
>
>
>         To:        [log in to unmask]
>         cc:
>         Subject:        Re: [TN] Cleaning paste when mis-aligned.
>
>
>
>       Cathy: This should not be a problem for the bare (unloaded) PCB.
> However if
>       you are doing a double sided reflow and   misprint the second side
> you need
>       to verify that the first side components are compatible with the
> ultrasonics
>       you are using.
>
>
>       Regards
>
>       Michael Barmuta
>
>       Staff Engineer
>
>       Fluke Corp.
>
>       Everett WA
>
>       425-446-6076
>
>       -----Original Message-----
>       From: Cathy Killen [mailto:[log in to unmask]]
>       Sent: Friday, October 26, 2001 7:30 AM
>       To: [log in to unmask]
>       Subject: [TN] Cleaning paste when mis-aligned.
>       Importance: High
>
>
>       Hello All & the mountain dew man.
>       Can a mis-printed PCB be washed in a ultrasonic bath to remove all
> paste
>       particles?
>       Is there any danger of damaging innerlayers of PCB?
>
>       Thanks in advance.
>
>       Cathy Killen
>       Training Instructor
>       Smtek Europe Ltd.
>       The information contained in the E-mail is confidential. It is
> intended only
>       for the stated addressee(s) and access to it by any other person is
>       unauthorised.
>       The views expressed in this E-mail are those of the author, and do
> not
>       represent the views of Smtek Europe, its associates or subsidiaries,
> unless
>       otherwise expressly indicated.
>       Please note: It is your responsibility to scan this E-mail for
> viruses.
>
>
> --------------------------------------------------------------------------
> --
>       -----
>       Technet Mail List provided as a free service by IPC using LISTSERV
> 1.8d
>       To unsubscribe, send a message to [log in to unmask] with following
> text in
>       the BODY (NOT the subject field): SIGNOFF Technet
>       To temporarily halt delivery of Technet send the following message:
> SET
>       Technet NOMAIL
>       Search previous postings at: www.ipc.org > On-Line Resources &
> Databases >
>       E-mail Archives
>       Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
>       information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700
>       ext.5315
>
> --------------------------------------------------------------------------
> --
>       -----
>
>
> --------------------------------------------------------------------------
> -------
>       Technet Mail List provided as a free service by IPC using LISTSERV
> 1.8d
>       To unsubscribe, send a message to [log in to unmask] with following
> text in
>       the BODY (NOT the subject field): SIGNOFF Technet
>       To temporarily halt delivery of Technet send the following message:
> SET Technet NOMAIL
>       Search previous postings at: www.ipc.org > On-Line Resources &
> Databases > E-mail Archives
>       Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
>       information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
>
> --------------------------------------------------------------------------
> -------
>
>
>
>

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2